Bend Test

Sonaspection has produced a range of bend test samples that can show a student or technician the impact welded defects can have on the structural integrity of a welded joint. We supply them in batches of 5 bars (12mm x 10mm x 200mm long) Each bar has 1 defect in it.
Lack of fusion flaws
Item Thickness
SV Plate 12mm
SV Plate 15mm
SV Plate 20mm
Cracks
Item Thickness
SV Plate 12mm
SV Plate 15mm
SV Plate 20mm
Sonaspection has produced a range of bend test samples that can show a student or technician the impact welded defects can have on the structural integrity of a welded joint. We supply them in batches of 5 bars (12mm x 10mm x 200mm long) Each bar has 1 defect in it.
  • Bar 1 LoSWF
  • Bar 2 Slag
  • Bar 3 Clear
  • Bar 4 LoRF
  • Bar 5 Toe Crack
Each bar is bend unlit the weld starts to fail and the defect is exposed.